I can provide pictures from when it was stirped down, sanded, new glass laid, a total of 3 layers, with the final layer being woven glass. After all the glass was layed I gave it 4 days to harden before sanding. After hours of sanding and prep work, I rolled a layer of COAT-IT on the bottom. Which is a an expoy with kevlar and graphite in it. The graphite of course making for a much more slicker bottom.

As I said, If you want I can send you before and after pictures.

just shoot me an e-mail or give me a call.